High temperature wear behavior of the surface-modified externally cooled rolls
(Elsevier, 2018)
Externally cooled rolls of a steel plant were coated using three different surface modification techniques, namely titanizing, boronizing and borotitanizing. The grown coatings were examined using optical microscopy, ...
Properties and Corrosion Behavior of Chromium and Vanadium Carbide Composite Coatings Produced on Ductile Cast Iron by Thermoreactive Diffusion Technique
(ASME, 2020)
Ductile iron (DI) owes many of its attractive mechanical properties to the graphite nodules in its structure. However, since galvanic coupling can occur between the graphite nodules and the matrix in aggressive environments, ...
Properties and tribological performance of ceramic-base chromium and vanadium carbide composite coatings
(Elsevier, 2019)
In the current study, the surface of AISI D2 steel was coated with the powder blends of ferro-vanadium (Fe-V) and ferro-chromium (Fe-Cr). The coatings were performed using a thermo-reactive diffusion (TRD) treatment by the ...
A new approach to sintering and boriding of steels "Boro-sintering": Formation, microstructure and wear behaviors
(Elsevier, 2020)
In this study, sintering and boriding methods are applied as a single step, and it is aimed to gain time and economic advantage. For this purpose, powder mixtures prepared in suitable compositions were subjected to sintering ...
Microstructure and mechanical properties of borided CoCrFeNiAl0.25Ti0.5 high entropy alloy produced by powder metallurgy
(Elsevier, 2021)
CoCrFeNiAl0.25Ti0.5 high entropy alloy alloys (HEA), produced by powder metallurgy were subjected to boriding to improve their mechanical properties. Sintering was carried out at 1200 degrees C for 2 h in Ar, and boriding ...
Effect of the boriding environment on the wear response of laser-clad AlCoCrFeNi high entropy alloy coatings
(Elsevier, 2022)
Laser-clad AlCrFeCoNi high entropy alloy (HEA) coatings, produced on the surface of AISI 316 L stainless steel, were pack-borided at 1000 °C for 4 h in open air, high-purity Ar and vacuum environments. The HEA, which had ...