A new approach to sintering and boriding of steels "Boro-sintering": Formation, microstructure and wear behaviors
(Elsevier, 2020)
In this study, sintering and boriding methods are applied as a single step, and it is aimed to gain time and economic advantage. For this purpose, powder mixtures prepared in suitable compositions were subjected to sintering ...
Microstructural, wear and corrosion characteristics of boronized AISI 904L superaustenitic stainless steel
(Elsevier, 2021)
AISI 900 series stainless steels are considered as low-cost alternatives to nickel-based superalloys used for highly corrosive environments. However, in terms of mechanical properties, they have average strength and hardness ...
Characteristics, high temperature wear and oxidation behavior of boride layer grown on nimonic 80A Ni-based superalloy
(Elsevier, 2021)
Nickel-based superalloy Nimonic 80A was pack-borided in a solid medium at temperatures of 850 degrees C and 950 degrees C for 2 h and 4 h using silicon-free boriding powders. To investigate the effects of the boriding ...
TTribocorrosion behavior of boronized Co1.19Cr1.86Fe1.30Mn1.39Ni1.05Al0.17B0.04 high entropy alloy
(Elsevier, 2021)
Boride layers were grown on the surface of a Co1.19Cr1.86Fe1.30Mn1.39Ni1.05Al0.17B0.04 high-entropy alloy (HEA) by boronizing at temperatures of 900, 950 and 1000 degrees C for 4 h using nanosized boronizing powders. ...
Characteristics, high temperature wear and oxidation behavior of boride layer grown on nimonic 80A Ni-based superalloy
(Elsevier, 2021)
Nickel-based superalloy Nimonic 80A was pack-borided in a solid medium at temperatures of 850 degrees C and 950 degrees C for 2 h and 4 h using silicon-free boriding powders. To investigate the effects of the boriding ...
Effect of the boriding environment on the wear response of laser-clad AlCoCrFeNi high entropy alloy coatings
(Elsevier, 2022)
Laser-clad AlCrFeCoNi high entropy alloy (HEA) coatings, produced on the surface of AISI 316 L stainless steel, were pack-borided at 1000 °C for 4 h in open air, high-purity Ar and vacuum environments. The HEA, which had ...