Microstructural, wear and corrosion characteristics of boronized AISI 904L superaustenitic stainless steel
(Elsevier, 2021)
AISI 900 series stainless steels are considered as low-cost alternatives to nickel-based superalloys used for highly corrosive environments. However, in terms of mechanical properties, they have average strength and hardness ...
TTribocorrosion behavior of boronized Co1.19Cr1.86Fe1.30Mn1.39Ni1.05Al0.17B0.04 high entropy alloy
(Elsevier, 2021)
Boride layers were grown on the surface of a Co1.19Cr1.86Fe1.30Mn1.39Ni1.05Al0.17B0.04 high-entropy alloy (HEA) by boronizing at temperatures of 900, 950 and 1000 degrees C for 4 h using nanosized boronizing powders. ...
Microstructure, some mechanical properties and tribocorrosion wear behavior of boronized Al0.07Co1.26Cr1.80Fe1.42Mn1.35Ni1.10 high entropy alloy
(Elsevier, 2021)
High-entropy alloys (HEAs) with face-centered cubic (FCC) structures exhibit high toughness and corrosion resistance, but their average strengths and relatively low wear resistance can limit their engineering ap-plications. ...
Effect of Cr Addition on Properties and Tribological Behavior at Elevated Temperature of Boride Layers Grown on Borosintered Powder Metallurgy Alloys
(Korean Institute of Metals and Materials, 2022)
This study focused on chromium addition (0 wt%, 3 wt%, 6 wt%, 9 wt% and 12 wt%) on the boride layer formation, microhardness, fracture toughness and elevated temperature friction and wear behaviour of alloys formed by ...
Determination of fracture toughness of boride layers grown on Co1.21Cr1.82Fe1.44Mn1.32Ni1.12Al0.08B0.01 high entropy alloy by nanoindentation
(Elsevier, 2022)
Multiphase boride layers consisting of (CoFe)2B, (Fe0.4Mn0.6)B, Cr2Ni3B6 and (Cr0.4Mn0.6)B were formed on the surface of Co1.21Cr1.82Fe1.44Mn1.32Ni1.12Al0.08B0.01 high entropy alloy by powder-pack boronizing at 900 °C, 950 ...