Effect of Different Arc Welding Processes on the Metallurgical and Mechanical Properties of Ramor 500 Armor Steel
(Asme, 2020)
In the present study, Ramor 500 armor steel plates were automatically welded using cold metal transfer arc welding (CMT), gas metal arc welding (GMAW), and hybrid plasma arc welding (HPAW) methods. To investigate the effects ...
Microstructural, wear and corrosion characteristics of boronized AISI 904L superaustenitic stainless steel
(Elsevier, 2021)
AISI 900 series stainless steels are considered as low-cost alternatives to nickel-based superalloys used for highly corrosive environments. However, in terms of mechanical properties, they have average strength and hardness ...
Effect of thermal degradation on the properties and wear behavior of Cr−V−C composite coatings grown on ductile iron
(Elsevier, 2021)
The thermal fatigue behavior of chromium vanadium carbide (Cr - V - C) coatings and the wear of the coatings after thermal fatigue cycling was studied. The Cr - V - C coatings were grown on the surface of a ductile iron ...
Microstructure, some mechanical properties and tribocorrosion wear behavior of boronized Al0.07Co1.26Cr1.80Fe1.42Mn1.35Ni1.10 high entropy alloy
(Elsevier, 2021)
High-entropy alloys (HEAs) with face-centered cubic (FCC) structures exhibit high toughness and corrosion resistance, but their average strengths and relatively low wear resistance can limit their engineering ap-plications. ...
Pack-Boriding of Monel 400: Microstructural Characterization and Boriding Kinetics
(Korean Institute of Metals and Materials, 2021)
Monel 400 was pack-borided in the temperature range of 1173-1273 K for exposure times of 2-6 h. The boride layers produced on the surface of the alloy were examined by scanning electron microscopy and phase identification ...
Effect of the boriding environment on the wear response of laser-clad AlCoCrFeNi high entropy alloy coatings
(Elsevier, 2022)
Laser-clad AlCrFeCoNi high entropy alloy (HEA) coatings, produced on the surface of AISI 316 L stainless steel, were pack-borided at 1000 °C for 4 h in open air, high-purity Ar and vacuum environments. The HEA, which had ...