Characterization of microstructure and high-temperature wear behavior of pack-borided Co-based Haynes 25 superalloy
(Elsevier, 2023)In this study, the effect of thermochemical boriding on the microstructural properties and high-temperature wear resistance of cobalt-based Haynes 25 superalloy was investigated. Haynes 25 alloy was subjected to a pack-boriding ...