Properties and High Temperature Dry Sliding Wear Behavior of Boronized Inconel 718
(Springer, 2020)
Silicide-free boride layers were grown on Inconel 718 Ni-based superalloy surface at 850 degrees C, 950 degrees C, and 1050 degrees C for 2, 4, 6 hour by the powder pack-boronizing process using nano-sized B4C powders. The ...
Microstructure and mechanical properties of borided CoCrFeNiAl0.25Ti0.5 high entropy alloy produced by powder metallurgy
(Elsevier, 2021)
CoCrFeNiAl0.25Ti0.5 high entropy alloy alloys (HEA), produced by powder metallurgy were subjected to boriding to improve their mechanical properties. Sintering was carried out at 1200 degrees C for 2 h in Ar, and boriding ...